(牙合)面厚度与肩台宽度连续变化的下颌第一磨牙全瓷冠三维有限元分析
  • ISSN号:1002-0098
  • 期刊名称:《中华口腔医学杂志》
  • 时间:0
  • 分类:R781.05[医药卫生—口腔医学;医药卫生—临床医学]
  • 作者机构:[1]第四军医大学口腔医学院修复科,西安710032, [2]西安电子科技大学机电工程学院
  • 相关基金:国家自然科学基金(30872907)
中文摘要:

目的 探讨(牙合)面厚度和肩台宽度同时连续变化情况下下颌第一磨牙全瓷冠的优化设计,以期为全瓷冠的临床设计提供理论基础.方法 运用逆向工程及计算机辅助设计技术建立(牙合)面厚度和肩台宽度连续变化的下颌第一磨牙三维有限元模型,设定(牙合)面厚度变化范围为1~3 mm,肩台宽度变化范围为0.4~1.2 mm,并在全瓷冠颊尖垂直向(牙合)面加载225 N的力,观察验面厚度和肩台宽度同时变化对全瓷冠、粘接剂、基牙、牙周膜和牙槽骨等效应力峰值的影响,同时进行灵敏度分析.结果 随着(牙合)面厚度和肩台宽度的增加,除牙周膜和牙槽骨的等效应力峰值无明显变化外,全瓷冠、粘接剂和基牙的等效应力峰值均下降.当(牙合)面厚度≥1.87 mm、肩台宽度≥0.66 mm时,全瓷冠、粘接剂和基牙的应力响应曲线斜率均位于-1~1之间,即在此区间内等效应力峰值变化相对较小.灵敏度分析显示,肩台宽度对全瓷冠和基牙等效应力峰值的影响较大,(牙合)面厚度对粘接剂等效应力峰值的影响较大.结论 在本项研究所设定的参数范围内,下颌第一磨牙全瓷冠的(牙合)面厚度应不小于1.87 mm,肩台宽度应不小于0.66 mm.

英文摘要:

Objective To investigate the effect of different occlusal thickness and shoulder finish line depth on stress distribution of all-ceramic crowns and to select optimal occlusal thickness and shoulder finish line depth using continuous variation of parameters. Methods This analysis was performed using mandibular first molar finite element modl. The range of occlusal thickness was set from 1 mm to 3 mm, and that of shoulder finish line depth was from 0. 4 mm to 1.2 mm. Load of 225 N was applied perpendicularly to the occlusal surface of the tooth at all buccal cusps to simulate functional occlusal force. The maximum equivalent stresses in crown, cement layer, abutment, periodontal ligament, alveolar bone were calculated, and the sensitivities of stresses to the variables were also evaluated. Results The maximum equivalent stresses in crown, cement layer and abutment decreased as occlusal thickness and shoulder finish line depth were increased, while no obvious change were found in maximum equivalent stresses in periodontal ligament and alveolar bone. When occlusal thickness exceeded 1.87 mm and shoulder finish line depth exceeded 0. 66 mm,the tangent slope rate of the maximum equivalent stress response curves ranged from - 1 to 1. Data indicated that occlusal thickness played a more important role in reducing maximum equivalent stress in cement layer than finish line depth did, and shoulder finish line depth was a more effective parameter in reducing maximum equivalent stress in crown and abutment than occlusal thickness was. Conclusions Occlusal thickness exceeding 1.87 mm and shoulder finish line depth exceeding 0. 66 mm are optimal design for ceramic crown on mandibular first molar from biomechanical point of view.

同期刊论文项目
同项目期刊论文
期刊信息
  • 《中华口腔医学杂志》
  • 北大核心期刊(2011版)
  • 主管单位:中国科协
  • 主办单位:中华医学会
  • 主编:
  • 地址:北京市东四西大街42号
  • 邮编:100710
  • 邮箱:cjst1953@cma.org.cn
  • 电话:010-85158254/5/6/7
  • 国际标准刊号:ISSN:1002-0098
  • 国内统一刊号:ISSN:11-2144/R
  • 邮发代号:2-64
  • 获奖情况:
  • 中国科协优秀科技期刊评比二等奖(1996),第二届全国优秀科技期刊评比三等奖(1996),入选“中国期刊方阵(双效期刊)”(2001)
  • 国内外数据库收录:
  • 美国化学文摘(网络版),荷兰文摘与引文数据库,美国生物医学检索系统,日本日本科学技术振兴机构数据库,中国中国科技核心期刊,中国北大核心期刊(2004版),中国北大核心期刊(2008版),中国北大核心期刊(2011版),中国北大核心期刊(2014版),中国北大核心期刊(2000版)
  • 被引量:24337