An innovative process of blast furnace (BF) operation involving charging with low-titanium vanadium-titanium magnetite carbon composite hot briquette (LVTM-CCB) was proposed for utilizing LVTM and conserving energy, In this study, the effect of LVTM-CCB charging ratio on the softening, melting, and dripping behaviors of the mixed burden was explored systemically, and the migration of valu- able elements V and Cr was extensively investigated. The results show that with increasing LVTM-CCB charging ratio, the softening inter- val T40 - T4 increases from 146.1℃ to 266.1℃, and the melting interval To - Ts first decreases from 137.2℃ to 129.5℃ and then increases from 129.5℃ to 133.2℃. Moreover, the cohesive zone becomes narrower and then wider, and its location shifts slightly downward. In addi- tion, the recovery ratios of V and Cr in dripped iron first increase and then decrease, reaching maximum values of 14.552% and 28.163%, respectively, when the charging ratio is 25%. A proper LVTM-CCB charging ratio would improve the softening--melting behavior of the mixed burden; however, Ti(C,N) would be generated rapidly in slag when the charging ratio exceeds 25%, which is not favorable for BF op- eration. When considering the comprehensive softening-melting behavior of the mixed burden and the recovery ratios of V and Cr, the rec- ommended LVTM-CCB charging ratio is 20%.