研究了粉煤灰混凝土(Fly ash concrete,FAC)、大掺量矿物掺合料混凝土(Concrete with high content mineral admixture,HCMC)和绿色高耐久性混凝土(Green high durable concrete,GHDC)在(5%MgCl2+5%Na2SO4)复合溶液中的长期侵蚀作用与干湿循环作用下的化学腐蚀行为。结果表明,在复合溶液的长期侵蚀作用下,GHDC具备比较好的抗腐蚀性能;在复合溶液的干湿循环作用下,HCMC的抗腐蚀能力比较强。因此,GHDC适合于长期的侵蚀环境中,而HCMC则更加适合于干湿交替的严酷条件。
The durability of fly ash concrete ( FAC), concrete with high contem mineral admixture (HCMC) and green high durable concrete (GHDC) subjected to the composite solution (5% MgCl2 + 5% Na2SO4 ) under long-term attack and dry-wet circulation were studied. Results show that GHDC has high durability subjected to the composite solution under long-term attack; HCMC has the best performance under dry-wet circu- lation. So GHDC is suitable for long-term attack, and HCMC is suitable for dry-wet circulation.