利用X射线衍射法分析了高炉渣中的非晶态和晶态含量,高炉渣(主要成分为w(CaO)38.2%,w(SiO2)35.7%,w(Al2O3)16.3%,w(MgO)8.3%)中晶态与非晶态含量的定量比例系数为0.70。
The quantificational analysis for the non-crystalline and the crystalline solids in blast furnace (BF) slag was conducted with X-ray diffraction method. The quantificational coefficient between the crystalline and the noncrystalline solids (the main composition of BF slag used: CaO 38.2 %, SiO2 35.7 %, Al2O3 16.3 %, MgO 8. 3 % ) is 0.70.