以聚合物光子晶体光纤空气孔阵列为模板,制备了Ag微米管阵列修饰的聚合物光子晶体光纤.讨论了银氨溶液和葡萄糖溶液浓度以及反应时间和温度对银微米管形貌的影响.在Ag(NH3)2^+与C6H6O浓度比为2,反应时间为20min,温度为65℃条件下光纤孔洞表面获得了规则的Ag微米管状结构,并对Ag的生长机理进行了讨论.
Silver microtube modified microstructured polymer optical fibres are prepared on the templates of hole arrays in MPOF. Effects of the concentration of Ag(NH3)2^+-glucose and the reaction time on the thickness of Agmicrotube are investigated. When Ag(NH3 )2^+ /glucose is two and the reaction time is 20 min, the smooth Ag-MPOF composite fibres are obtained at 65℃.