Y-a-sialon ceramics with different compositions were hot-press sintered.Varying the m or n value in the a-Sialon general formula,both the a-sialon grain morphology and phase assemblages present diversification,therefore,affecting the toughness and hardness.Meanwhile,varying the compositional parameters also influenced the composition and structure of the intergranular glass phase,as well as its oxidation behavior at 1100e1200℃.The oxidation of the intergranular phase M0in the Y-a-sialon ceramics was significantly enhanced with further rising the oxidation temperature to 1300℃.
Y-α-sialon ceramics with different compositions were hot-press sintered. Varying the m or n value in theα-Sialon general formula, both the α-sialon grain morphology and phase assemblages present diversification, therefore, affecting the toughness and hardness. Meanwhile, varying the compositional parameters also influenced the composition and structure of the intergranular glass phase, as well as its oxidation behavior at 1100-1200 ℃. The oxidation of the intergranular phase Mt in the Y-α-sialon ceramics was significantly enhanced with further rising the oxidation temperature to 1300 ℃.